Brand Name : Victory
Model Number : Inconel 718
Certification : ISO9001 ROHS
Place of Origin : China
MOQ : 30 Kg
Price : Negotiable
Payment Terms : L/C, T/T, Western Union, MoneyGram
Supply Ability : 300 tons per month
Delivery Time : 20~40 Days
Packaging Details : Spool Carton box, Coil package with polybag,then in woodencase
Name : AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components
Material : Nickel Chromium Iron
Ni (Min) : 50~55%
Density : 8.24 g/cm3
Melting point : 1260-1320°C
Elongation (≥ %) : 25 %
Thermal conductivity : 15.9 W/m·K
Finishing : Bright,Oxided, acid white
Application : Construction, Industry Oil, piping systems
Yield strength : 550MPa
Tensile strength : 910 MPa
Hardness : ≤ 363 HB
Standard : ASTM, ASME
size : 6~200mm
shape : Round, Square, flat
Advantages of Inconel 718 Strips
High Strength-to-Weight Ratio: Provides durability without adding excessive weight.
Excellent Fabricability: Can be easily machined and formed into complex shapes.
Resistance to Oxidation and Corrosion: Ensures longevity in challenging environments.
Applications of Inconel 718 Strips
Aerospace Components
Thrust Reversers: Used in thrust reversers for jet engines, where high-temperature resistance and strength are essential.
Structural Components: Fabricated into various structural parts that require lightweight yet strong materials.
Oil and Gas Industry
Downhole Equipment: Employed in valves, fittings, and other components exposed to harsh environments.
Subsea Applications: Ideal for use in subsea pipelines and connectors due to its excellent corrosion resistance.
Nuclear Applications
Fuel Rods and Structural Supports: Used in nuclear reactors where materials must withstand extreme conditions.
Marine Applications
Components in Marine Engines: Suitable for various parts exposed to seawater, where corrosion resistance is vital.
High-Performance Engineering
Fasteners and Bolts: Can be used to manufacture bolts and fasteners that require superior mechanical properties.
Heat Exchangers
Heat Exchanger Tubes: Utilized in heat exchangers where high temperatures and corrosive fluids are present.
Chemical Properties of Inconel 718
Nickel (plus Cobalt) .......................................................50.00-55.00
Chromium......................................................................17.00-21.00
Iron .....................................................................................Balance
Niobium (plus Tantalum)....................................................4.75-5.50
Molybdenum .....................................................................2.80-3.30
Titanium.............................................................................0.65-1.15
Aluminum ..........................................................................0.20-0.80
Cobalt ...............................................................................1.00 max.
Carbon..............................................................................0.08 max.
Manganese .......................................................................0.35 max.
Silicon ...............................................................................0.35 max.
Phosphorus.....................................................................0.015 max.
Sulfur...............................................................................0.015 max.
Boron ..............................................................................0.006 max.
Copper..............................................................................0.30 max
Density | 8.19g/cm³ | 0.296 lb/in³ |
Melting point | 1260-1336 | 2437°F |
Inconel series
Customize size as below
Shape | Size(mm) |
WIre | 0.5-7.5 |
Rod/Bar | 8.0-200 |
Strip | (0.5-2.5)*(5-180) |
Tube | custom made |
Plate | custom made |
contact us
email:victory@dlx-alloy.com
Oem service:
Welcome customized size
We are experience factory for OEM&ODM service
![]() |
AMS 5596 ASTM B670 superalloy nickel alloy 718 inconel 718 strip for aerospace Components Images |